What happens inside the material
Almost everything expands when heated. If a part can expand freely and uniformly, no stresses develop. The problem appears when expansion is restrained or uneven, and internal stresses then arise. When these exceed the local strength, a crack starts, and it propagates if the energy released allows it to.
Main causes
- Differential expansion: two bonded materials, such as a resin around a metal insert, have different expansion coefficients. When the temperature changes, one pushes against the other.
- Thermal gradients or thermal shock: a rapid change heats or cools the surface before the interior. In brittle materials such as ceramics and glass, this mechanism is a typical cause of fracture.
- Residual stresses: from curing, molding or cooling, which add to the thermal stresses.
- Aging: under prolonged heat, the polymer loses plasticizers, oxidizes and becomes more brittle, so it tolerates less strain.
- Cycling: repeated variations cause thermal fatigue and cracks that grow little by little.
What the crack looks like depending on its origin
Radial cracks around an insert point to differential expansion. A network of fine surface cracks suggests a thermal gradient or aging of the outer layer. A single clean fracture in a ceramic indicates thermal shock or impact. Cracks that start at sharp corners point to stress concentration caused by the design.
Electrical consequences
An internal crack is an air void with partial discharges; a surface crack retains moisture and contamination. In both cases the insulating capability drops even though the material, in principle, is still sound.
What can be done
- Select materials with compatible expansion coefficients.
- Round corners and avoid abrupt changes in cross section.
- Control heating and cooling rates.
- Check the service temperature against the material’s rating.
What to check first
Find where the crack starts and what is at that point. The origin is almost always at an interface or a change in geometry.