Why silicon is vulnerable
Crystalline silicon is a brittle material. A cell is a fraction of a millimeter thick, and a crack starting from an edge or a solder joint can propagate with little energy. The cell does not bend like a metal; when the stress exceeds what it can tolerate in an area with a defect, it cracks.
Where the stresses come from
- Handling and transport: vibration, impacts, incorrect stacking of the modules.
- Installation: stepping on the modules, overtightening the clamps or mounting them on an uneven structure.
- Wind and snow loads, which flex the module repeatedly.
- Daily thermal cycles, which expand and contract materials with different coefficients and concentrate stress at the solder joints.
- Hail and other impacts.
What consequences the crack has
A crack does not always reduce power immediately. The damage depends on whether it isolates part of the cell from the metal contacts. An isolated area stops contributing and forces the rest to conduct more current. Over time, cycling can open the crack and the loss grows. A partially isolated cell can also give rise to a hot spot.
How they are detected
They are not usually visible to the naked eye. Electroluminescence, which makes the cell emit light by passing a current through it in the dark, shows inactive areas and crack traces. The I-V curve can show a loss of current or fill factor, but does not locate the cause. Thermography reveals cells with anomalous behavior.
How to reduce the risk
This is achieved through careful handling and mounting practices, well-leveled structures, modules designed to distribute stress, and inspection on receipt and after installation. A cracked cell does not always call for immediate replacement; the decision depends on the extent of the inactive area and how it evolves.