Why does an insulator lose properties with moisture?

An insulator loses properties with moisture because water, which is polar and carries dissolved ions, penetrates the material or adsorbs on its surface, increasing conductivity, permittivity and losses and reducing surface resistance.

The underlying cause

Water is a highly polar molecule with high permittivity, and it almost always carries dissolved ions from salts and contaminants. A dry insulator has few mobile charges. When it takes up water, ionic conduction paths and dipoles that respond to the field appear, and the electrical properties change.

Observable effects

  • Higher permittivity: water contributes its own polarization, and in a mixture it raises the effective value.
  • Higher dielectric losses: from relaxation of the water dipoles and from ionic conduction.
  • Lower resistivity: in the volume and, above all, at the surface, where a moist film with salts creates a leakage path.
  • Lower breakdown voltage and greater risk of tracking: the conductive film concentrates the field and promotes discharges.

How water gets in

By diffusion through the volume in hygroscopic materials, by capillary action along fibers or interfaces in laminates, and through microcracks. In composite materials, the interface between fiber and resin is usually the fastest route. Some matrices, such as certain polyesters, can undergo hydrolysis, which breaks chains and permanently degrades strength.

Mechanical and dimensional effects

Water plasticizes some polymers, lowers their glass transition temperature and makes them swell. Cycling humidity and temperature generates stresses that open cracks and delaminate interfaces, which lets more water in.

What the engineer sees

Equipment that passes when dry and fails in a humid environment, leakage currents that increase with relative humidity, losses that drift during the first hours of a test, or partial recovery after drying. If recovery is incomplete, there is irreversible damage.

What to check first

  1. Conditioning state of the sample.
  2. Surface cleanliness.
  3. Water absorption of the material and quality of the interface.