What is defined before starting
The result depends entirely on the conditions, so the protocol must set them: temperature, charge and discharge current, depth of discharge, voltage limits, rest periods and the end-of-life criterion, such as a percentage of the initial capacity. Without that, results are not comparable.
Required equipment
A battery cycler is used, or a combination of power supply and electronic load able to control current and voltage precisely, with logging of voltage, current and temperature, and a thermal chamber to keep the temperature stable. It must have safety limits that stop the test under abnormal conditions.
Test procedure
- Initial characterization: reference capacity and internal resistance.
- Cycling with the defined profile, repeating charge, rest and discharge.
- Periodic capacity and resistance checks using a reference procedure, at fixed cycle intervals.
- Continuing until the end-of-life criterion or an agreed number of cycles is reached.
What is obtained
The curve of capacity versus number of cycles and the evolution of internal resistance. Capacity usually falls slowly and may then accelerate toward the end, so the shape of the curve matters more than a single point. The loss is due to reactions at the electrodes and the growth of surface layers.
How to interpret with care
Cycles with higher current, greater depth or extreme temperature accelerate wear, and the results apply only to the conditions tested. In addition, aging also occurs over time without cycling, known as calendar aging, which is studied with separate tests. Extrapolating to service life requires additional models and data.
Notice
Batteries under test can heat up, vent gases or catch fire if they fail. The test must be performed by qualified personnel, with adequate protection, ventilation and emergency procedures.