24/7 emergencies 814 777 6921812 230 6079WhatsApp 811 786 0768
Electrónica MonterreyElectrónica MonterreyLaboratorios Creativeit Talk to an engineer
Menu

How are the cells in a pack balanced?

Cells are balanced by equalizing their state of charge: the passive method dissipates energy from the highest cells in resistors, and the active method transfers it between cells.

Why they become unbalanced

In a series pack the same current flows through all the cells, but no two are identical. They have slightly different capacities and different self-discharge, and they run at different temperatures depending on their position. Over the cycles these differences accumulate and the states of charge spread apart. Since charging ends when the highest cell reaches its limit and discharging ends when the lowest cell reaches its own, the weakest cell defines the usable energy of the entire pack.

Passive balancing

The battery management system connects a resistor in parallel with the highest cells, and the diverted current is dissipated as heat while the others keep charging. It is simple, inexpensive and robust. Its limitation is that it wastes energy and the balancing current is small, so correcting a large spread takes a long time.

Active balancing

Instead of dissipating, it transfers charge from the high cells to the low ones using capacitors, inductors or transformers. It makes better use of the energy and can also act during discharge, but it adds complexity, components and points of failure.

When it is applied

Most strategies balance at the end of charging, when a cell’s voltage clearly relates to its state of charge. In chemistries with a very flat voltage curve, such as lithium iron phosphate, voltage says little in the middle of the range, which is why effective balancing happens near the extremes.

What the engineer sees in practice

  • A cell voltage spread that grows with cycling indicates imbalance or differences in internal resistance.
  • A cell in the same position that always drops first may point to a thermal or connection problem, not just a capacity problem.
  • If balancing runs continuously and fails to close the gap, the cell probably has higher self-discharge or a defect.

Balancing does not recover lost capacity: it only keeps the weakest cell from limiting the pack further. Measuring and handling traction packs requires qualified personnel and the applicable safety procedures.

We do real tests, on video! Watch them on our YouTube channel →

Do you have a problem nobody has been able to measure?

Talk directly to the engineer in charge, with no middlemen.

Talk to an engineer