Why the layers are the weak point
A laminate withstands loads in the plane of its fibers very well, but between layers it is held together only by the resin. The interlaminar strength and the fracture toughness between layers are much lower. Delamination is therefore the most characteristic failure mode of these materials.
What causes it
- Out-of-plane stresses: bending, free edges, holes and thickness changes concentrate stresses that separate the layers.
- Impact: can leave internal damage that is barely visible on the surface.
- Voids and poor impregnation: air pockets or dry areas are starting points.
- Moisture: weakens the interface between fiber and resin; on freezing or heating, trapped water generates pressure.
- Thermal cycling: the difference in expansion between fiber and matrix, and between layers of different orientation, generates repeated stresses.
- Poor curing or contamination: a poorly bonded interface soon gives way.
How it progresses
It begins with microcracks in the matrix or at the interface, which join up and advance between layers. While the laminate is under load, the debonded area grows. It can take a long time to show on the surface, as a bulge or a hollow sound when tapped.
Electrical consequences
In printed circuit boards, delamination creates air voids that facilitate discharges, trap moisture and break vias or traces. In high-voltage insulators, these voids are sites of partial discharges.
How to detect it
- Tap test, which identifies hollow areas by the change in sound.
- Ultrasound, which locates reflections in the debonded area.
- Metallographic sections to observe the interface.
- For circuit boards, thermal cycling tests and via resistance tests.
How to prevent it
Control the cure, dry the material before processing, avoid unprotected edges and holes, and limit thermal cycling. Check moisture and bond quality first.