The direct answer
It is almost never “the seal” as a concept that fails; a specific entry path fails. Water finds the weakest route, and that route may be the main gasket, a cable gland, a screw, a membrane, an enclosure seam or a pore in the material.
Most frequent causes
- Inadequate compression: an over-compressed gasket deforms permanently; an under-compressed one leaves gaps. The groove geometry and part tolerances determine how much it is compressed.
- Material and aging: elastomers that harden with heat or ozone, or that deform under prolonged load, lose their sealing capacity.
- Cable entries: a cable that does not match the seal diameter, or insufficient tightening, is a common leak.
- Screws and through holes: without their own seal, they are a direct path.
- Surfaces: burrs, scratches or injection flash on the sealing face.
Pressure and temperature
A closed enclosure contains air. If the product heats up and then cools, or cools suddenly on contact with water, the internal pressure drops relative to the external pressure and can draw water in through marginal seals. That is why a water test after thermal exposure is more demanding than one with the part at room temperature. Many designs include a vent membrane to equalize pressure.
How to diagnose it
An air leak test is run to locate the path, dye is added to the water, or moisture-sensitive absorbent paper is placed inside. Check where the water appears first. The gasket is also examined for contact marks, which show whether compression was uniform.
What to correct
Depending on the cause: redesign the groove or the gasket material, control tolerances, change the cable gland, seal the screws or add venting. The test is then repeated with the same assembly and verified against the designation you intend to declare.
When it is not a seal problem
An enclosure that is porous as manufactured, such as cast or printed parts, can let water through the material itself.