Polarization mechanisms
When an alternating electric field is applied, a material polarizes through several mechanisms with different response times:
- Electronic: deformation of the electron clouds; this is the fastest and follows the field up to optical frequencies.
- Atomic or ionic: relative displacement of atoms or ions, also very fast.
- Dipolar: orientation of polar groups in the chains, much slower and dependent on temperature and molecular mobility.
- Interfacial: accumulation of charge at boundaries between phases, free charges or additives; the slowest, relevant at low frequencies.
What happens as frequency rises
At low frequency all the mechanisms contribute and the real permittivity is higher. As the frequency increases, each mechanism stops following the field when its characteristic time exceeds the period, and the permittivity drops in a step. In that region energy is dissipated as heat, which appears as a maximum in the imaginary part of the permittivity (losses). The two effects are linked: the dispersion of the real part and the loss peak are manifestations of the same relaxation.
Polar and nonpolar polymers
Nonpolar polymers such as polyethylene, polypropylene or PTFE show little dispersion and nearly constant permittivity over a wide range. Polar polymers, such as PVC, polyamides and many epoxy resins, show marked relaxations, and their permittivity and losses vary considerably with frequency.
Effect of temperature and moisture
As temperature rises, chain mobility increases and the relaxation peaks shift toward higher frequencies. Near the glass transition the dipolar response changes greatly. The absorption of water, which has a high permittivity, raises permittivity and losses, especially in hygroscopic polymers. At very low frequencies, conduction through impurities increases the apparent losses.
What the engineer sees in practice
A curve of permittivity and loss factor against frequency, at several temperatures. The material is chosen according to the operating frequency: high-frequency circuits call for stable permittivity and low losses; for power insulation at power frequency, what matters is that losses do not grow with aging and moisture. The measurement frequency and temperature are always reported.