How Does Solid Insulation Age Under Electrical Stress?

Solid insulation ages under electrical stress through cumulative damage: partial discharges in voids erode the material, branching channels (trees) form, and the sound thickness shrinks until breakdown occurs.

Damage that accumulates

Solid insulation rarely fails because its dielectric strength is exceeded on the first day. More commonly, moderate stress sustained over years and combined with other factors causes microscopic damage that grows until breakdown. This is why its life depends on the stress level: the higher the field, the shorter the time.

Main mechanisms

  • Partial discharges: in voids, delaminations or interfaces, the local field exceeds what the contained gas can withstand and produces repeated discharges. Each discharge bombards the walls with ions and electrons and releases chemical byproducts such as ozone and acids that attack the material.
  • Electrical treeing: starting from a point of field concentration, such as a sharp point or a void, branching channels grow that penetrate the insulator and reduce the useful thickness.
  • Water treeing: in polymeric insulation exposed to moisture and field, branching structures containing water form and progressively weaken the material.
  • Thermal degradation: heat, from dielectric losses or from current, accelerates the chemical reactions that embrittle the material.
  • Mechanical stress and thermal cycling: these create cracks and separations where discharges start.

Factors that combine

In practice, engineers speak of thermal, electrical, environmental and mechanical stresses acting together. Wet, hot insulation ages faster under the same electric field. Surface contamination, radiation, chemicals and vibration add to the damage. None of these factors acts in isolation.

What the engineer sees

  1. An increase in partial discharge activity over time.
  2. A change in tan delta or capacitance.
  3. Gases in the oil or around the insulation, depending on the equipment.
  4. Sudden failure after an overvoltage event on insulation that was already weakened.

How to interpret the result

Partial discharge and dielectric loss measurements detect deterioration before failure, and their trend matters more than a single reading. Activity is evaluated relative to the operating voltage and compared with similar equipment.

When it does not apply

Liquid and gaseous insulation can recover after a discharge, or can be treated and replaced. The aging described here is specific to solids, which do not self-heal.

Warning: tests and measurements at elevated voltage must be performed by qualified personnel, in accordance with applicable regulations.

We do real tests, on video! Watch them on our YouTube channel →

Do you have a problem nobody has been able to measure?

Talk directly to the engineer in charge, with no middlemen.

Talk to an engineer