Two kinds of loss
Degradation modes are grouped into loss of lithium inventory, which is lithium that can no longer take part, and loss of active material, which is electrode material that can no longer host lithium. Both reduce capacity. A third effect, the rise in internal resistance, reduces the available power even if capacity does not change as much.
The main mechanisms
- SEI layer growth: a protective layer forms on the anode from the electrolyte. With each cycle it cracks and re-forms, consuming lithium and increasing resistance.
- Lithium plating: with fast charging, low temperatures or saturated anodes, some of the lithium deposits on the surface instead of intercalating. This lithium is lost and can form structures that damage the separator.
- Cathode degradation: cracking from volume change, structural changes and dissolution of transition metals.
- Mechanical stress: the electrodes swell and contract with each cycle and lose contact with the current collector.
Factors that accelerate wear
High temperature accelerates side reactions. Keeping the battery at a high state of charge for long periods also promotes them, so calendar aging occurs even without use. Large depths of discharge and high currents add wear per cycle.
How it looks in the laboratory
In a cycling test, measured capacity decreases and resistance grows. The voltage curve changes shape and differences appear between the cells in a pack. Diagnostic tests, such as low-rate capacity and resistance measurement, help determine whether lithium loss or material loss dominates.
These ideas explain why manufacturers limit the usable state-of-charge window and manage temperature. How long a specific battery lasts depends on its design and use, and must be evaluated with data from the cell.