How is a battery characterized with an electronic load?

The battery is discharged with an electronic load at controlled current, power or resistance while voltage, current and time are logged, down to a defined voltage limit; from this you obtain the capacity, the discharge curve and the internal resistance.

What the test yields

Discharging the battery in a controlled way shows its delivered capacity, the shape of the voltage-versus-time curve and the voltage drop when current is applied, which reflects its internal resistance. The results depend on the procedure, so they should only be compared between tests performed under the same conditions.

General procedure

  1. Condition: start from a known state of charge, normally a full charge according to the method for the battery chemistry, then let it rest and allow the temperature to stabilize.
  2. Choose the mode: constant current is the most common for obtaining capacity; constant power imitates electronic loads; constant resistance, simple loads.
  3. Set the cutoff limit: the minimum voltage recommended by the manufacturer, so as not to damage the battery by over-discharge. The electronic load must have a cutoff function configured.
  4. Log: voltage at the battery terminals, with separate sensing to avoid the drop in the cables, current and time, and temperature.
  5. Calculate: capacity is the integral of current over time, and energy, the integral of power.

Internal resistance

When a current step is applied, the voltage drops immediately because of the internal resistance, and then continues to fall more slowly because of electrochemical processes. The ratio of the voltage jump to the current step gives an estimate of the resistance, which depends on temperature, state of charge and measurement time.

What you see in practice

  • The higher the discharge current, the lower the usable capacity and the greater the voltage drop.
  • At low temperature, capacity and voltage decrease.
  • The voltage partially recovers when the discharge is interrupted.

How to interpret the result

A capacity below the rated value may indicate aging, but also incomplete prior conditioning or a test current different from the reference current.

Precautions

Batteries store a great deal of energy and can heat up, catch fire or release gases in the event of a short circuit or abuse. Tests, especially with lithium or high-voltage batteries, must be performed by qualified people with suitable protection and in accordance with the applicable regulations.

We do real tests, on video! Watch them on our YouTube channel →

Do you have a problem nobody has been able to measure?

Talk directly to the engineer in charge, with no middlemen.

Talk to an engineer