What the Arrhenius acceleration factor is

The Arrhenius acceleration factor expresses how many times faster a chemical or degradation process occurs at an elevated temperature than at the use temperature, according to an activation energy characteristic of the mechanism.

The relationship

Many degradation processes, such as oxidation, diffusion or chemical reactions in polymers and insulators, proceed at a rate that grows exponentially with temperature. Svante Arrhenius described that dependence: the rate is proportional to an exponential term containing the activation energy divided by the product of the Boltzmann constant and the absolute temperature.

The acceleration factor

When two temperatures are compared, the use temperature and the test temperature, the ratio of the rates is the acceleration factor. It depends on the activation energy, which is specific to each mechanism, and on the difference between the reciprocals of the absolute temperatures. The higher the activation energy, the more the same temperature rise accelerates the process.

What this means in practice

  • Temperatures must be used in kelvin, never in degrees Celsius, within the equation.
  • Two materials with different activation energies accelerate differently under the same test.
  • A small uncertainty in the activation energy produces a large uncertainty in the factor.

Where the activation energy comes from

It must not be assumed. It is obtained from tests at several temperatures, by plotting the logarithm of the rate or of the life against the reciprocal of the absolute temperature. If the points line up, the model applies and the slope gives the energy. If they curve or change slope, there is more than one mechanism or a material limit has been exceeded.

What the engineer sees

The typical result is a table of equivalent times between the test temperature and the use temperature. A short test at high temperature translates into a long time at normal temperature, with the caveat that the value is an estimate.

Limits

It describes only thermally activated processes. It does not cover failures dominated by humidity, mechanical stress or thermal cycling, which require other models or a combination. In addition, near material transitions, such as the glass transition or melting, the model ceases to be valid. Validity must be justified case by case.